Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 80.7 MPa | 11700 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength at Break | 80.7 MPa | 11700 psi | ASTM D638 |
Chase Plastics CP Pryme® N100HSL (DAM) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 80.7 MPa | 11700 psi | ASTM D638 |
Chase Plastics CP Pryme® N100L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |