Mechanical Properties Metric English Comments
Tensile Strength at Break 41.4 - 55.2 MPa
6000 - 8000 psi
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound
BMC 610 molding compound is a mineral filled, glass­ fiber­ reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact..
Tensile Strength at Break 41.4 - 55.2 MPa
6000 - 8000 psi
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..