Polymer Property : Tensile Strength at Break = 85100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 587 MPa
85100 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 401
Characteristics:Braze 401 is an intermediate temperature filler metal that may be used as a cadmium free substitute for Easy-Flo 30 or used in applications where an intermediate silver-copper-zinc ..
Tensile Strength at Break >= 587 MPa
>= 85100 psi
12 lb. Minimum Tensile Load 0.0134 in. Diameter
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 12 lb
Information provided by Shakespeare Company.