Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.07 MPa | 880 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8201-67W228 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tensile Strength at Break | 6.07 MPa | 880 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tensile Strength at Break | 6.07 MPa | 880 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4755A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.07 MPa | 880 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4764A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.07 MPa | 880 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 181-55MED Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. .. |