Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.087 MPa | 1318 psi | ASTM D 412 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |