Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.60 MPa | 1390 psi | ISO R 527 |
Stir SpA SPI 65 (PVC) Application: PlugsInformation provided by STIR SpA |
|||
Tensile Strength at Break | 9.60 MPa | 1390 psi | ASTM D638 |
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de.. |