Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.96 MPa | 1440 psi | After 72hr/177°C air oven, ASTM D573 |
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont. |