Polymer Property : Tensile Strength at Break = 900 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 530 - 900 MPa
76900 - 131000 psi
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head..