Tensile Strength at Break 947.3 MPa
137400 psi
Hardwire 12x-23-12 High Density Tape
The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformabi..