Polymer Property : Tensile Strength at Break = 9560 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.9 MPa
9560 psi
3M Scotch® 3072 Recycled Corrugated Tape
Scotch® Recycled Corrugate Tapes can be applied by hand for low volume packing with a hand-help tape dispenser or with a 3M-Matic™ Case Sealer for high productivity packing.Information provided by..