Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.172 MPa @Strain 300 % |
25.0 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 0.172 MPa @Strain 300 % |
25.0 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP-2137 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |