Mechanical Properties Metric English Comments
Tensile Stress 1.21 MPa

@Strain 300 %,
Temperature 23.0 °C
175 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p..
Tensile Stress 1.21 MPa

@Strain 300 %
175 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP1192A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.21 MPa

@Strain 300 %
175 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2285CMT Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.21 MPa

@Strain 300 %
175 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2830E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..