Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 78.0 MPa | 11300 psi | |
Lehmann & Voss LUVOCOM® 1105/TF/20/BN PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Tensile Stress | 77.7 MPa @Strain 8.87 %, Temperature -20.0 °C |
11300 psi @Strain 8.87 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |