Mechanical Properties Metric English Comments
Tensile Stress 96.0 MPa
13900 psi
Lehmann & Voss LUVOCOM® 1105-7740 PEEK, lubricant modified, heat stabilized
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Tensile Stress 96.0 MPa
13900 psi
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG