Polymer Property : Tensile Stress = 150 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1736R1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1870-CR Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2207 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2241 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1128 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2825E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2830C CLR Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2830 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 1.03 MPa

@Strain 300 %
150 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..