Polymer Property : Tensile Stress = 16.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 16.7 MPa
2420 psi
at Break, MD; ASTM D882
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene
LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industria..