Tensile Stress 13.1 MPa

@Strain 300 %
1900 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-2696A Thermoplastic Elastomer
Uses: Cell Phones; Consumer Applications; General Purpose; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes..