Polymer Property : Tensile Stress = 2.62 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.62 MPa

@Strain 300 %
380 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer
Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p..