Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 225 MPa | 32600 psi | |
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Tensile Stress | 225 MPa | 32600 psi | |
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Tensile Stress | 225 MPa | 32600 psi | |
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Tensile Stress | 225 MPa | 32600 psi | |
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Tensile Stress | 225 MPa | 32600 psi | |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Tensile Stress | 225 MPa | 32600 psi | |
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |