Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 265 MPa | 38400 psi | |
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Tensile Stress | 265 MPa | 38400 psi | |
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis.. |
|||
Tensile Stress | 265 MPa | 38400 psi | |
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |