Polymer Property : Tensile Stress = 30500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1105-7442 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 20-8283 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1/CF/20 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1/CF/20/HS Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1/CF/20/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys..
Tensile Stress 210 MPa
30500 psi
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..