Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 255 MPa | 37000 psi | |
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Tensile Stress | 255 MPa | 37000 psi | |
Lehmann & Voss LUVOCOM® 1-7488 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Tensile Stress | 255 MPa | 37000 psi | |
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Tensile Stress | 255 MPa | 37000 psi | |
Lehmann & Voss LUVOCOM® 1105/XCF/15-S PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |