Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.60 MPa

@Strain 100 %
667 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-80W175 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for ..
Tensile Stress 4.60 MPa

@Strain 100 %
667 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..