Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 280 MPa | 40600 psi | |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Tensile Stress | 280 MPa | 40600 psi | |
Lehmann & Voss LUVOCOM® 1105-8179 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Tensile Stress | 280 MPa | 40600 psi | |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Tensile Stress | 280 MPa | 40600 psi | |
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Tensile Stress | 280 MPa | 40600 psi | |
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |