Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 52.0 MPa | 7540 psi | |
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |