Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-79W233 Thermoplastic Elastomer A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |