Polymer Property : Tensile Stress = 550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.79 MPa

@Strain 100 %
550 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Stress 3.79 MPa

@Strain 300 %
550 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1658A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 3.79 MPa

@Strain 300 %
550 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1766 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 3.79 MPa

@Strain 300 %
550 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..