Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.00 MPa @Strain 1.00 %, Time 3.60e+6 sec |
580 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Tensile Stress | 4.00 MPa @Strain 100 % |
580 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles,.. |