Mechanical Properties Metric English Comments
Tensile Stress 6.70 MPa

@Strain 100 %
972 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..