Mechanical Properties Metric English Comments
Tensile Stress 48.0 MPa
6960 psi
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Tensile Stress 48.0 MPa
6960 psi
Lehmann & Voss LUVOCOM® 80-7718 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Tensile Stress 48.0 MPa
6960 psi
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Tensile Stress 48.0 MPa
6960 psi
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..