Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 77.0 MPa | 11200 psi | |
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |