Tensile Stress 9.00 MPa
1310 psi
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable ..