Polymer Property : Tensile Stress = 900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.21 MPa

@Strain 300 %
900 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 6.21 MPa

@Strain 300 %
900 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2112 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 6.21 MPa

@Strain 300 %
900 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2860M-CR Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 6.21 MPa

@Strain 300 %
900 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2990 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 6.21 MPa

@Strain 300 %
900 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 6.21 MPa

@Strain 300 %
900 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2890M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..