Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 92.0 MPa | 13300 psi | |
Lehmann & Voss LUVOCOM® 1105-7741 PEEK, with mineral filler, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Tensile Stress | 92.0 MPa | 13300 psi | |
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Tensile Stress | 92.0 MPa | 13300 psi | |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |