Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 93.0 MPa | 13500 psi | |
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Tensile Stress | 93.0 MPa | 13500 psi | |
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |