Mechanical Properties Metric English Comments
Modulus of Rigidity 71.0 GPa
10300 ksi
H.C. Starck NRC® 91 Tantalum - 7% Tungsten Alloy
Applications: NRC® 91 Metal wire products are primarily used for their superior tensile and yield strengths and torsion modulus. These properties are retained at high temperatures in vacuum. F..