Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | 1.0 t @Thickness <=3.17 mm |
1.0 t @Thickness <=0.125 in |
Bend Severity 90°, specimens at least 1" by 2", transverse direction |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |
|||
Bend Radius, Minimum | 1.0 t @Thickness <=1.02 mm |
1.0 t @Thickness <=0.0400 in |
Bend Severity 180°, specimens at least 1" by 2", transverse direction |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |