Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | 2.0 t @Thickness <=4.75 mm |
2.0 t @Thickness <=0.187 in |
Bend Severity 90°, specimens at least 1" by 2", transverse direction |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |
|||
Bend Radius, Minimum | 2.0 t @Thickness <=2.03 mm |
2.0 t @Thickness <=0.0800 in |
Bend Severity 180°, specimens at least 1" by 2", transverse direction |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |