Polymer Property : Charpy Impact Unnotched = 1.37 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.37 J/cm²

@Temperature -20.0 °C
6.52 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis MD231U Polypropylene Compound, Mineral Filled
MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc..