Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 10.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -20.0 °C
10.9 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -20.0 °C
10.9 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -20.0 °C
10.9 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -20.0 °C
10.9 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder
FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
Charpy Impact Unnotched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant
Information provided by Polykemi AB
Charpy Impact Unnotched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber
PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smo..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® S RV250FR (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced
Radiflam® B is a range of flame retardant polybutylene terephthalate (PBT) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided ..