Polymer Property : Charpy Impact Unnotched = 13.4 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 13.4 J/cm²

@Temperature -30.0 °C
63.8 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66  (Unverified Data**)
Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers