Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 13.5 J/cm² @Temperature 23.0 °C |
64.2 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6HM PA6 PA 6 for compounding, basic type, modified for general use, used in the automotive, electrical, engineering and consumer goods industry. Delivered in natural color - white (contains TiO2)Information.. |
|||
Charpy Impact Unnotched | 13.5 J/cm² @Temperature -40.0 °C |
64.2 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | 13.5 J/cm² @Temperature 23.0 °C |
64.2 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BM 25 FN20 700350 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen |
|||
Charpy Impact Unnotched | 13.5 J/cm² @Temperature 23.0 °C |
64.2 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BM 25 FN20 DUS013 000000 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen, optimized for laser marking at 1064 nm, |