Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 14.3 J/cm² @Temperature -40.0 °C |
68.1 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | 14.3 J/cm² @Temperature 23.0 °C |
68.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |