Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.30 J/cm² @Temperature 23.0 °C |
15.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature 23.0 °C |
15.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -20.0 °C |
15.7 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -20.0 °C |
15.7 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature 23.0 °C |
15.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -20.0 °C |
15.7 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 79 GF 20 Polypropylene Homopolymer, 20% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH303G20 is a 20% glass filled Polypropylene - Homopolymer injection molding grade with good stiffness.Information provided by SAX Polymers |