Polymer Property : Charpy Impact Unnotched = 19.5 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 19.5 J/cm²

@Temperature 23.0 °C
92.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® DP BC 310 EF 600065 Nylon 6
PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow)