Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 21.0 J/cm² @Temperature 23.0 °C |
99.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Charpy Impact Unnotched | 21.0 J/cm² @Temperature -30.0 °C |
99.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
Charpy Impact Unnotched | 21.0 J/cm² @Temperature -30.0 °C |
99.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Charpy Impact Unnotched | 21.0 J/cm² @Temperature -30.0 °C |
99.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Charpy Impact Unnotched | 21.0 J/cm² @Temperature -30.0 °C |
99.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Charpy Impact Unnotched | 21.0 J/cm² @Temperature -20.0 °C |
99.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |