Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 23.0 J/cm² @Temperature -30.0 °C |
109 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1700 000000 PBT PBT, non-reinforced, extrusion, food contact |
|||
Charpy Impact Unnotched | 23.0 J/cm² @Temperature -30.0 °C |
109 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
Charpy Impact Unnotched | 23.0 J/cm² @Temperature 23.0 °C |
109 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |
|||
Charpy Impact Unnotched | 23.0 J/cm² @Temperature -30.0 °C |
109 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Charpy Impact Unnotched | 23.0 J/cm² @Temperature -30.0 °C |
109 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® N2320 0035 POM Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF |