Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.30 J/cm²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra..
Charpy Impact Unnotched 5.30 J/cm²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A RCF3505 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 5.30 J/cm²

@Temperature -30.0 °C
25.2 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 5.30 J/cm²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styron INSPIREâ„¢ DLGF 9621.00 Compounded Polypropylene, 60% LGF
Overview: DLGF 9621.00 is a polypropylene homopolymer reinforced with 60% by weight of long glass fiber. PP-LGF60, Long Glassfiber Granulate). DLGF 9621.00 is produced by pultrusion/melt-impregnatio..
Charpy Impact Unnotched 5.30 J/cm²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF
Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion..
Charpy Impact Unnotched 5.30 J/cm²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1fU
Styron LGF 9621 Homopolymer Polypropylene
Overview: LGF 9621 is polypropylene homopolymer reinforced with 60% by weight of long glass fibers. (PP-LGF60, Long Glass fiber Granulate). This PP-LGF60 is a ‘concentrate’ which has to be..
Charpy Impact Unnotched 5.30 J/cm²

@Temperature -30.0 °C
25.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced
SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers
Charpy Impact Unnotched 5.30 J/cm²

@Temperature -30.0 °C
25.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1fU
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Charpy Impact Unnotched 5.30 J/cm²

@Temperature 23.0 °C
25.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..