Polymer Property : Charpy Impact Unnotched = 29.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.20 J/cm²

@Temperature 23.0 °C
29.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled
Flame retardant, RoHS compliantInformation provided by PolyPlastic Group.
Charpy Impact Unnotched 6.20 J/cm²

@Temperature 23.0 °C
29.5 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® A RV250AF (cond.) Nylon 66-25GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
Charpy Impact Unnotched 6.20 J/cm²

@Temperature -30.0 °C
29.5 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A ECP3808 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 6.20 J/cm²

@Temperature -30.0 °C
29.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
Charpy Impact Unnotched 6.20 J/cm²

@Temperature -30.0 °C
29.5 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A RV400 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 6.20 J/cm²

@Temperature -30.0 °C
29.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
Charpy Impact Unnotched 6.20 J/cm²

@Temperature -30.0 °C
29.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..