Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 31.0 J/cm² @Temperature -30.0 °C |
148 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta.. |